A-1 Wire Tech, Inc.
INCONEL® ALLOY X750

A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with high tensile and creep-rupture properties at temperatures to about 1300ºF (700ºC). Its excellent relaxation resistance is useful for high-temperature springs and bolts. Used in gas turbines, rocket engines, nuclear reactors, pressure vessels, tooling, and aircraft structures. Standard product forms are round, flats, extruded section, forging stock, plate, sheet, strip, pipe, tube, and wire.

Typical Mechanical Properties

Limiting Chemical Composition, %

Nia - 70.0 min.
Cr - 14.0-17.0
Fe - 5.0-9.0
Ti - 2.25-2.75
Al - 0.40-1.00
Nbb - 0.70-1.20
C - 0.08 max.
Mn - 1.00 max.
Si - 0.50 max.
S - 0.01 max.
Cu - 0.50 max.
Coc - 1.00 max.
aPlus Co.
bPlus Ta.
cIf determined.

Typical Mechanical Properties
(Precipitation Hardened)

Rupture Strength (1000 h)


1100ºF / 595ºC••••••
1200ºF / 650ºC••••••
1350ºF / 730ºC••••••
1500ºF / 815ºC••••••
psi
92,000
68,000
37,000
16,000
MPa
630
470
260
110

Physical Constants and Thermal Properties

Density, Ib/in3 •••••• 0.299
g/cm3 •••••• 8.28
Melting Range, °F •••••• 2540 – 2600
°C ••••••1390 – 1430
Specific Heat, Btu/lb •°F •••••• 0.103
J/kg • °C •••••• 431
Curie Temperature, °F •••••• -193
°C •••••• -125
Permeability at 200 Oersted (15.9 kA/m) •••••• 1.0035
Coefficient of Expansion, 70 – 200°F, 10-6 in/in • °F •••••• 7.0
21 – 93°C, μm/m • °C •••••• 12.6
Thermal Conductivity, Btu • in/ft2•h•°F •••••• 83
W/m• °C •••••• 12.0
Electrical Resistivity, ohm• circ mil/ft •••••• 731
μΩ•m •••••• 1.22

Specifications and Designation

UNS N07750
BS HR505
ASTM B 637
ASME SB-637,
Boiler Code Section III
Werkstoff Nr. 2.4669
SAE AMS 5542, 5582, 5583,
5598, 5667-5671, 5698,
5699, 5747, 7246
MIL-N-7786,
MIL-N-8550,
MIL-S-23192,
MIL-N-24114
NACE MR-01-75
AFNOR NC 15 FeT